dc.description.abstractEste trabalho analisa a variação da classificação de resistência ao fogo de um sistema de selagem para proteção de tubulação de PVC de 100 mm de diâmetro para a Curva de Crescimento Lenta (EN 13381-8). Portanto, partese da pergunta: Qual a redução da classificação de resistência ao fogo dos sistemas de selagem para tubulações de PVC de 100 mm dentro de cavidades das paredes ou forros? Argumenta-se que a classificação de resistência ao fogo da selagem destas tubulações pode ter variação, pois estão expostos à diferentes taxas de aquecimento ao estarem localizadas dentro de cavidades de paredes e forros. Este trabalho justifica-se socialmente pelo uso crescente de selagem nas edificações residenciais e comerciais do Brasil, em que ensaios destes sistemas de proteção no Brasil são escassos. Por outro lado, busca-se contribuir academicamente fornecendo análise de sistemas intumescentes de selagem em curva de crescimento lenta. Obteve-se resultados a partir de dois ensaios de resistência ao fogo de um mesmo sistema de selagem certificado exposto na curva ISO-834 e Curva de Crescimento Lenta. Embora o sistema ensaiado foi aprovado para as duas curvas, observou-se que houve variações no critério de isolamento da classificação de resistência ao fogo. Quanto maior a taxa de aquecimento, maior a temperatura na face fria até o fechamento da abertura pelo material intumescente.pt_BR
dc.description.abstractThis work analyzes the variation of the fire resistance classification of a firestop system for the protection of 100 mm diameter PVC pipes for the Smouldering Curve (EN 13381-8). Therefore, it starts with the question: What is the reduction of the fire resistance rating of the firestop systems for PVC pipes of 100 mm inside cavities of the walls or ceilings? It is argued that the fire resistance rating of the firestop of these pipes may vary, as they are exposed to different heating rates when located within cavities of walls and ceilings. This work is socially justified by the increasing use of firestop in residential and commercial buildings in Brazil, in which tests of these protection systems in Brazil are scarce. On the other hand, it seeks to contribute academically by providing analysis of intumescent firestop systems in a smouldering curve. Results were obtained from two tests of fire resistance of the same certified firestop system exposed to the ISO-834 curve and Smouldering Curve. Although the tested system was approved for both curves, it was observed that there were variations in the insulation criteria of the fire resistance classification. The higher the heating rate, the higher the temperature on the cold face until the opening is closed by the intumescent material.en
dc.format.mimetypeapplication/pdfpt_BR
dc.language.isoporpt_BR
dc.rightsOpen Accessen
dc.subjectFirestopen
dc.subjectEngenharia civilpt_BR
dc.subjectFire resistance testen
dc.subjectIncêndiospt_BR
dc.subjectSegurançapt_BR
dc.subjectExperimental testen
dc.subjectSmouldering fire curveen
dc.subjectIntumescent systemsen
dc.titleAvaliação de sistema de selagem intumescente em curva de incêndio com crescimento lentopt_BR
dc.title.alternativeEvaluation of intumescent firestop system in smouldering fire curve en
dc.typeTrabalho de conclusão de especializaçãopt_BR
dc.identifier.nrb001121877pt_BR
dc.degree.grantorUniversidade Federal do Rio Grande do Sulpt_BR
dc.degree.departmentEscola de Engenhariapt_BR
dc.degree.localPorto Alegre, BR-RSpt_BR
dc.degree.levelespecializaçãopt_BR
dc.degree.specializationCurso de Especialização em Engenharia de Segurança Contra Incêndiospt_BR


Thumbnail
   

Este item está licenciado na Creative Commons License

Mostrar registro simples